Existing buildings
Cracks in walls: cosmetic or structural? When to worry
How to tell a plaster crack from a structural one: what crack widths mean, diagonal cracks, cracks in beams and columns, and when to call an engineer.
Most cracks in the walls of a house or building are cosmetic. They are fine cracks in plaster caused by shrinkage, heat or moisture, and they do not affect the safety of the building. A crack needs an engineer when it is wide, diagonal or tapering, keeps growing, or appears in a beam, column or slab.
Why walls crack
A material cracks when the stress in it exceeds its strength. SP 25, the Bureau of Indian Standards handbook on cracks, sorts cracks into two groups:
- Structural cracks come from incorrect design, faulty construction or overloading. They may endanger the building.
- Non-structural cracks come from materials shrinking, swelling, heating and cooling. They generally do not weaken the structure.
Non-structural cracks still need proper repair, since rain entering through them can corrode the steel in nearby concrete.
Which cracks are usually cosmetic?
- Fine, map-like cracks in plaster. Plaster shrinks as it dries, more so when the mix is rich or curing was poor. These cracks appear in the first dry spell after construction. Plaster that sounds hollow when tapped has lost its bond with the wall.
- A straight vertical crack where a wall meets a concrete column. Concrete and masonry move differently, and the joint opens a few months after construction.
- A horizontal crack at the top of the walls on the top floor. The roof slab expands and bows upward in the sun and shifts the walls below. Filled with hard mortar, this crack tends to return.
What does a diagonal crack in a wall mean?
A diagonal crack has more than one possible cause. Concrete lintels cast on site shrink as they dry, and over wide openings this can cause diagonal cracks running upward from the lintel ends, usually in the first dry spell after construction.
Uneven settlement of the foundation, typically at a corner, causes diagonal cracks that are wider at the top and run through the plinth into the foundation. Signs that point towards ground movement are:
- a crack wider at one end than the other
- a stepped crack following the mortar joints
- a crack that shows on both faces of the wall
- a crack that continues below the plinth
The UK’s National House-Building Council (NHBC) advises having any diagonal or stepped crack checked, whatever its width, and so do we.
Is a crack in a beam or column serious?
Always have an engineer look at a crack in a beam, column or slab. SP 25 cites extensive cracking of a concrete beam as an example of structural cracking.
Reinforced concrete is designed to keep cracks very fine. IS 456, the Indian concrete code, generally limits design crack widths to 0.3 mm, and to 0.2 mm or less where the member is exposed to weather or moisture. The wall-crack table below does not apply to these members.
Corroding reinforcement shows as a straight crack along the line of a bar, rust stains, or concrete flaking off to expose the steel. Rust takes up more space than steel, so it cracks the concrete and then pushes the cover off. SP 25 describes these cracks appearing 10 to 25 years after construction, earlier in thin sunshades with inadequate cover.
How wide is too wide?
Wall cracks are often graded using BRE Digest 251, from the UK’s Building Research Establishment.
| Category | Typical width | What it usually indicates |
|---|---|---|
| 0, negligible | under 0.1 mm | Hairline cracks. No action needed. |
| 1, very slight | up to 1 mm | Fine cracks, dealt with during normal redecoration. |
| 2, slight | up to 5 mm | Easily filled. Doors and windows may stick slightly. |
| 3, moderate | 5 to 15 mm, or several over 3 mm | Cracks need cutting out and patching. Doors and windows stick. Rain may get in. |
| 4, severe | 15 to 25 mm, depending on the number of cracks | Extensive repair. Frames distort, floors slope, walls lean or bulge. |
| 5, very severe | usually over 25 mm | Major repair or partial rebuilding. Danger of instability. |
BRE treats categories 0 to 2 as aesthetic, 3 and 4 as affecting how the building works, and 5 as a stability problem. SP 25 uses a simpler scale: thin cracks are under 1 mm, medium cracks 1 to 2 mm, and wide cracks over 2 mm.
The scale was developed for low-rise masonry buildings, and width is only one part of the picture. Position, direction, the number of cracks and whether a crack is growing also matter.
How climate and ground cause cracks in Indian buildings
- Monsoon wetting and drying. Porous walling such as brick, laterite, concrete block and mortar swells when wet and shrinks as it dries.
- Flat roofs in strong sun. The top of a concrete roof slab gets much hotter than its underside, so the slab arches up and moves outward. SP 25 recommends an insulating or protective layer over the slab, which it notes is common practice in hot countries like India.
- Humid air. SP 25 notes that relative humidity above 75 percent, as in coastal areas, causes rapid corrosion of reinforcement. IS 456 classes concrete exposed to severe rain or a coastal environment as “severe” exposure.
- Shrinkable clay. On black cotton soil, a shallow foundation moves as the soil swells in the rains and shrinks in dry weather.
- Soft or filled ground. Where fill is poorly compacted, settlement can begin when water from heavy rain or flooding reaches the foundation.
Several often act together on one site. We describe how we design for them in Engineering for India’s conditions.
What to do before you call
Record the crack before anyone fills or paints over it.
- Photograph it with a ruler beside it, close up and from further back.
- Measure the widest point in millimetres.
- Mark both ends with a pencil line and the date.
- Make a pencil mark on each side of the crack and measure the distance between them. If that distance changes, the crack is moving.
- Check again every few weeks for several months, after heavy rain, and at different times of day. Cracks caused by heat open and close with the temperature.
- Look at the other face of the wall.
- Note sticking doors or windows, sloping floors, damp patches, leaking pipes or drains, digging next door, large trees nearby, or a recent flood.
- Note when the building was built, any additions, and when you first saw the crack.
SP 25 advises against repairing cracks that are still developing. Fill a crack once it has stopped moving, using a flexible sealant for cracks that move with the seasons.
When to involve a structural engineer
Ask an engineer to inspect the building if:
- a wall crack is wider than about 5 mm at any point
- a crack is diagonal, stepped or tapering
- a crack shows on both faces of the wall or runs through the plinth
- a crack has grown since you first marked it
- there is any crack in a beam, column, slab, sunshade or balcony, or rust staining or loose concrete
- doors and windows stick, floors slope, or walls lean or bulge
- cracks appeared after a flood or after digging nearby
- you plan to add a floor to a building that has cracks
An engineer reads the crack pattern with the building’s history and ground, and checks for ongoing movement, often with tell-tales fixed across the cracks. Repair follows the cause. A thermal crack needs a flexible joint and better roof protection. A settlement crack is filled only after the movement has been dealt with.
Adding a floor to an existing building is part of our structural engineering work. If you are unsure about a crack, contact an engineer with your photographs and notes, and we will tell you whether it needs a visit.
Sources
- SP 25:1984, Handbook on causes and prevention of cracks in buildings (BIS): causes and types of cracks, crack patterns, corrosion, roof slab movement, tell-tales and repair.
- IS 456:2000, Plain and reinforced concrete (BIS): design crack width limits (clause 35.3.2) and exposure classes (Table 3).
- Assessing cracks in houses (BRE, 2014): BRE Digest 251 categories and their aesthetic, serviceability and stability groups.
- HS2 Information Paper C3: Ground settlement (UK Government): Table 1.1 crack widths and damage descriptions, and the note that width alone does not measure damage.
- Cracking in your home (NHBC, 2025): causes of cracks in homes and when to have one checked.
Common questions
Should I fill a crack before an engineer sees it?
No. Take photographs, measure it and mark its ends with the date first. Filler and paint hide the evidence of whether the crack is still moving.
Are cracks in a new house normal?
Fine cracks in plaster, and at joints between concrete and masonry, often appear in the first dry season as the materials shrink. Wide, diagonal or growing cracks in a new house are not normal and should be checked.
Why does a crack come back after painting?
Cracks caused by heat or moisture open and close with the seasons, so a rigid filler cracks again. They need a flexible sealant, and the cause, such as an unprotected roof slab, needs attention.
Is a crack in a beam or column dangerous?
It needs an engineer's inspection in every case. Rust stains or loose concrete near the crack can mean the steel inside is corroding.